Tom-
Tom, thanks for catching the units error. I fixed the script (attached below) to read the values as molal and that greatly improves the situation, but the values produced manually still do not replicate the values reported via the script.
For example, the "manual" model yields
Hematite 3.7604s/sat
Goethite 1.3588s/sat
Jarosite-K -2.5521
Fe(OH)3(ppd) -2.7895
While the script yields
Hematite 3.187
Goethite 1.072
Jarosite-K -3.295
Fe(OH)3(ppd) -3.077
For the first set of conditions in the jarosite.txt file. Any ideas??
-
Here is the Jarosite.text input file (attached)
-
Hello,
I'm trying to run multiple saturation index analyses for the first time in SpecE8 in version 7.0. I've managed to adapt the calcite example to work for my data and it will run (Jarosite script attached), however the mineral SIs reported in the ouput file are different than those calculated if I manually input the data into SpecE8 (jarosite basis attached). The differences are small if I run the model at 25 C, but become very significant at T=50.
Can anyone point me towards a solution or explanation?